US 3,669,907 A#5992464 Most CitedExpiredUnited States (USPTO)Utility

Semiconductive elements

15Forward Citations (#5992464 Global)
0.3/yrCitation Velocity (#27028797 Global)
10.97Citation PageRank (#910603 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Semiconductive elements having a specific resistivity of the semiconductor range (that is, 105 to 108 ohm-cm) which have an ohmic resistance even in an considerably high electric field and are highly durable in adverse physical and atmospheric conditions, which are manufactured by heating a mixture of powder of vitreous binding material and powder of semiconductive metal oxide dispersed in the former powder. Further, the dielectric strength and the uniformity of resistivity of said semiconductive elements can be improved by adding, to the mixture, powder of an oxide whose conductivity is much higher than that of said semiconductive metal oxide.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 15.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 2Independent Claim

    A method for manufacturing a semiconductive element having particles of pulverized semiconductive metal oxide dispersed in a vitreous binding material, comprising the steps of mixing pulverized glass, whose average grain size is smaller than 1 micron, with a powder of at least one semiconductive metal oxide selected from the group consisting of SnO2, TiO2, WO3, Sb2O5, Cr2O3, Fe2O3, V2O5 and Bi2O3, whose average grain size is smaller than 5 microns but larger than the grain size of said glass, the amount of said metal oxide being 10 to 35 percent in volume; stirring the mixture with a volatile

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗