Method for the electrolytic removal of drawing or rolling lubricants on steel strands
Abstract
A one-step method for the removal of drawing or rolling lubricants from metal strands is described, in which the strands are subjected to an electrolytic treatment at a current density of 30-60 amps/in2 in an aqueous bath which contains about 6 to 16 wt. percent NaOH, .5 to 6% Na4P2O7 and .5 to 5% Na2CO3.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 2.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
The method of claim 1, in which the electrolyte is maintained at a temperature of 160* to 210* F and consists essentially of from 10 to 20 percent by weight of a mixture of 60 to 80% NaOH, 5 to 30% Na4P2O7 and 5 to 25% Na2CO3.
- Claim 3Depends on #2
The method of claim 2, in which the current is introduced to the strand via said electrolyte, and said current density is at least 45 amps/in2.
- Claim 4Depends on #3
The method of claim 3, in which the polarity of the strand is reversed as it passes through a series of treatment zones, with the polarity of the strands being anodic in the final treatment zone.