High modulus boron nitride fibers
Abstract
Boric oxide fibers having a maximum diameter of about 10 microns are heated in an ammonia atmosphere under such conditions as to produce partially nitrided fibers consisting essentially of B, N, O and H wherein the N is present to the extent of from about 35 percent to about 55 percent. The partially nitrided fibers are then heated in an inert atmosphere at a temperature of at least about 1800*C while simultaneously subjecting the fibers to sufficient longitudinal tension as to at least prevent longitudinal shrinkage of the fibers and preferably to cause elongation of the fibers during heating. The resulting fibers, consisting essentially of boron nitride, are of high purity and are characterized by a relatively high Young''s modulus of elasticity, which renders them especially suitable for reinforcing plastic, ceramic or metal matrices in the preparation of fiber reinforced composites.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 29.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
A yarn consisting of a plurality of fibers as set forth in claim 1.
- Claim 3Depends on #2
A yarn as set forth in claim 2 which consists essentially of continuous filaments.
- Claim 4Depends on #2
A yarn as set forth in claim 2 which consists essentially of staple fibers.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 29 total)
References Cited — Backward Prior Art (9)
Non-Patent Literature (1)
- The Vapor Phase Deposition of Refractory Materials, I. E. Campbell et al., Electrochemical Society Journal, Vol. 96, July Dec. 1949, pp. 318 333