Abstract

One side of a drawn homogeneous filament having at least 17 percent boiling water shrinkage is heated above its melting point while under high tension. The filament is then prebulked while under substantially no tension by being exposed to hot air at a temperature above the yarn glass transition temperature, soon after the initial heat treatment, and preferably before being wound. This produces a tighter crimp when the yarn is later subjected to hot water.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 5.

Claims (3 — 0 Independent, 3 Dependent)

  1. Claim 2Depends on #1

    The filament defined in claim 1, wherein r is within the range of 0.018 to 0.024 millimeter.

  2. Claim 3Depends on #1

    The filament defined in claim 1, wherein R is within the range of 0.1 to 0.14 millimeter.

  3. Claim 4Depends on #1

    The filament defined in claim 1, wherein P is in the range of 0.19 to 0.5 millimeter.