Electrical contact for silicon carbide members
Abstract
Tantalum and gold alloy electrical contacts are applied to selected areas of a body of silicon carbide. An oxidized surface is first produced on the silicon carbide body and removed from those portions of the surface to which the alloy contact of the body is to be applied. A thin layer of aluminum is deposited on only the oxidized surface. Thin films of tantalum and gold are alternately deposited on the exposed surface of the silicon carbide. Any tantalum and gold deposited on the aluminum forms an alloy which is readily removed by an etchant which attacks tantalum-gold-aluminum intermetallics but will not attack the tantalum-gold alloy electrical contact of the body.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 10.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
The process of claim 1 wherein the heat treating of the silicon carbide body with gold-tantalum layers present only on the selected areas is accomplished at a first elevated temperature of from 850* to 1,050* C. for a period of about 10 minutes and then heat treating the body at a second elevated temperature of from 1,500* to 1,700* C. for a period not exceeding about 15 seconds at the maximum temperature to alloy the tantalum, the gold, and the silicon carbide.
- Claim 3Depends on #2
The process of claim 2 wherein the etchant is a saturated solution of sodium hydroxide.
- Claim 4Depends on #3
The process of claim 3 including the process step prior to etching the silicon carbide body of heat treating the silicon carbide body at an elevated temperature of from 280* to 320* C. for a period of time of up to 16 hours.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗