Patents
US 3,661,658 A#5545070 Most CitedExpiredUnited States (USPTO)Utility

High-strength and high-toughness cast steel for propellers and method for making propellers of said cast steel

16Forward Citations (#5545070 Global)
0.3/yrCitation Velocity (#25400035 Global)
5.82Citation PageRank (#2591924 Global)
4Prior Art Cited
2Claims (0 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of making a high strength, high toughness cast steel marine propeller comprised of not more than 0.25 percent of carbon, not more than 1 percent of silicon, not more than 3 percent of manganese, from 5-20 percent of chromium, from 1-8 percent of cobalt, and from 0.5-7 percent of one or both of molybdenum and tungsten, and the remainder consisting of iron. In addition, the cast steel may contain up to 8 percent of nickel and up to 4 percent of copper, depending on the conditions. The method comprises casting the propeller into individual sections, welding said sections together, heating to a temperature of 800* to 1,000* C. and air cooling. The propeller can be aged by heating to a temperature between 450* and 700* C. If desired, the individual cast sections can be annealed prior to welding.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 16.

Claims (2 — 0 Independent, 2 Dependent)

  1. Claim 2Depends on #1

    A method as set forth in claim 1, wherein the individual sections are annealed at a temperature of 630*-700* C. prior to the welding step.

  2. Claim 3Depends on #2

    A method, as set forth in claim 2, comprising the further step of aging the welded casting at a temperature of 450*-600* C. to increase its strength subsequent to the slow cooling step.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗