Patents
US 3,661,564 A#2626756 Most CitedExpiredUnited States (USPTO)Utility

Extraction of cobalt and nickel from laterite

27Forward Citations (#2626756 Global)
0.5/yrCitation Velocity (#15138049 Global)
7.35Citation PageRank (#1766842 Global)
7Prior Art Cited
3Claims (0 Indep. · 3 Dep.)
0Drawings / Sheets

Abstract

A method for the recovery of nickel and cobalt from laterite with the elimination of iron, wherein the laterite is divided into a major and a minor portion and the minor portion is treated with hydrochloric acid to form a suspension. The major portion of laterite is mixed with the suspension to form a slurry which is roasted to form cobalt and nickel chloride. The nickel and cobalt chlorides are then dissolved by treating the solid residue with water, ferric chloride remaining in the residue. The solution is then subjected to a recovery treatment including cation exchange to separate the cobalt and nickel ions, and reduction to produce cobalt and nickel.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 27.

Claims (3 — 0 Independent, 3 Dependent)

  1. Claim 2Depends on #1

    A method according to claim 1, wherein the said high temperature treatment comprises drying followed by roasting at a temperature between 250* and 350* C., the duration of the said roasting being in the order of one to a few hours, wherein the hydrogen chloride is recycled so as to participate in the treatment of the minor fraction of the laterite, and wherein the concentration of chloride ions in the said suspension is comprised between 3 and 20 times the stoichiometric concentration necessary for transforming the nickel oxide initially contained in the major fraction of the laterite, into ni

  2. Claim 3Depends on #2

    A method according to claim 2, wherein a fraction of the mixture is recycled after drying and before roasting, in order to be mixed with the slurry with a view to adjusting its water content.

  3. Claim 4Depends on #1

    A method according to claim 1, wherein the s

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 27 total)

PatentTitleYearCitations
US 2007180953 A1High purity cobalt, method of manufacturing thereof, and high purity cobalt targets—6
US 5,428,990 AMethod of evaluation segregation of solid-liquid interface and segregation apparatus thereof19954
RU 2,149,910 C1METHOD OF NICKEL RECOVERY FROM Ni-Fe-Mg LATERINE ORE WITH HIGH CONTENT OF MAGNESIUM20007
WO 2007/087698 A1Hybrid process using ion exchange resins in the selective recovery of nickel and cobalt from leaching effluents—6
US 6,478,966 B2System for extracting tetrodotoxin200249
US 2004228783 A1Process for the recovery of value metals from material containing base metal oxides—55
US 4,382,082 ARecovery of cobalt values by absorption from ammoniacal solution19835
AU 2006203772 B2Process for Recovering Value Metal Species from Laterite-Type Feedstock20100
WO 2007/106969 A1Process for recovering value metal species from laterite-type feedstock—8
US 2009241731 A1System and method for extracting base metal values from oxide ores—17
US 3,871,978 AProcess for the production of high-purity metals from nickeliferous mattes19757
AU 2007211854 B2Hybrid process using ion exchange resins in the selective recovery of nickel and cobalt from leaching effluents20122
US 2008289448 A1Hybrid Process Using Ion Exchange Resins in the Selective Recovery of Nickel and Cobalt from Leaching Effluents—13
US 3,884,681 AProcess for the production of high-purity metals from nickeliferous mattes197513
US 6,485,542 B2Ni-Fe alloy sputtering target for forming magnetic thin films, magnetic thin film, and method of manufacturing the Ni-Fe alloy sputtering target200235