Refining of cubic boron nitride
Abstract
Cubic boron nitride is refined from a mixture of cubic boron nitride and hexagonal boron nitride by adding to the mixture lithium hydroxide, sodium hydroxide, or potassium hydroxide, or mixtures thereof and water as may be necessary to control the hydroxide fusion temperature, heating to a low-temperature molten state to dissolve the hexagonal boron nitride, and separating the cubic boron nitride from the remainder of the mixture.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 17.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 2Depends on #1
The method of claim 1 wherein the hydroxide temperature is about 300* C.
- Claim 3Depends on #1
The method of claim 1 wherein the hydroxide is sodium hydroxide.
- Claim 4Independent Claim
In the production of refined cubic boron nitride from a mixture containing cubic boron nitride and hexagonal boron nitride, the steps of dissolving the hexagonal boron nitride in a hydroxide molten at about 350* C selected from the group consisting of lithium, sodium, potassium, and mixtures thereof, and separating the solution from the cubic boron nitride.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 17 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2,947,617 A | Abrasive material and preparation thereof | 1960 | 104 |
| US 3,212,851 A | Boron nitride having a new structure | 1965 | 10 |