Patents
US 3,660,199 A#3325134 Most CitedExpiredUnited States (USPTO)Utility

Method of preventing measling when making epoxy laminates

23Forward Citations (#3325134 Global)
0.4/yrCitation Velocity (#18568946 Global)
11.76Citation PageRank (#810850 Global)
2Prior Art Cited
3Claims (0 Indep. · 3 Dep.)
0Drawings / Sheets

Abstract

Measling, the appearance of spots or stars under the surface of a resin portion of an epoxy-glass fiber laminate, is prevented or significantly diminished by a laminating process which includes curing plies of glass cloth and epoxy resin at an elevated temperature, e.g., 300* to 400* F., at an elevated pressure, e.g., 750 to 1,500 pounds per square inch, until gel formation occurs by reaction of the epoxy resin and curing agent, after which heating is continued at approximately the same temperature but at a lower pressure, e.g., 50 to 400 lbs./sq. in. Suitably, the initial curing step lasts for about 30 to 80 minutes and the subsequent step takes about 20 to 50 minutes, such times varying with the thickness of the laminate, the nature of the expoxy resin, the temperature employed, the geometry of the laminate, the type of reinforcing cloth, the curing apparatus used and the presence or absence of metal molded into the plastic. After completion of heating, the laminate is cooled in the press and is then removed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 23.

Claims (3 — 0 Independent, 3 Dependent)

  1. Claim 2Depends on #1

    A method according to claim 1 wherein the curing is of a plurality of epoxy resin-glass fiber laminae at a pressure over 700 lbs./sq. in. and is conducted over a period of about 30 to 80 minutes and the subsequent heating at a pressure of about 50 to 400 lbs./sq. in. is conducted for about 20 to 50 minutes.

  2. Claim 3Depends on #2

    A method according to claim 2 wherein the laminate contains at least three laminae and the cooling effected takes place within about 5 to 30 minutes and lowers the temperature of a middle lamina of the laminate to less than 150* F.

  3. Claim 4Depends on #3

    A method according to claim 3 wherein the epoxy resin is a diglycidyl ether of Bisphenol A, the curing agent is dicyandiamide and the glass sheet is a plain weave of chrome treated fibers.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (2)