Thin film nickel temperature sensor and method of forming
Abstract
Thin film nickel temperature sensors having a temperature coefficient of resistance of above +0.2 percent/* C and a resistance above 0.35 ohms per square are formed by electron beam evaporation of a high purity nickel source at pressures below 8 X 10 6 torr and deposition of the evaporated nickel atop a dielectric substrate, e.g. a polyimide film, heated above 60* C. The nickel film preferably is deposited to a thickness between 250 A and 3,000 A and masking is employed to produce a desired configuration in the deposited nickel film. To stabilize the resistance of the deposited nickel film, a dielectric encapsulant such as alumina, silica, a polyimide or a fluorocarbon then is overlayed upon the film by conventional vacuum deposition or bonding techniques.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 19.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
A method of forming a temperature sensor according to claim 1 wherein said substrate is a polyimide heated to a temperature between 150* C and 300* C and said nickel is evaporated in a vacuum less than 1 X 10 6 torr.
- Claim 3Depends on #2
A method of forming a temperature sensor according to claim 2 wherein said source is deposited at a rate greater than 30 A per second to a thickness between 750 A and 1,500 A.
- Claim 4Depends on #1
A method of forming a temperature sensor according to claim 1 further comprising the steps of: depositing a dielectric encapsulating layer atop said nickel film.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗