Patents
US 3,660,031 A#4719135 Most CitedExpiredUnited States (USPTO)Utility

Method for preparing boron suboxide

18Forward Citations (#4719135 Global)
0.3/yrCitation Velocity (#22553484 Global)
7.91Citation PageRank (#1563947 Global)
0Prior Art Cited
2Claims (0 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Boron suboxide (B7O) is prepared by the reduction of zinc oxide with boron in an inert atmosphere at a temperature of 1,200*1,500* C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 18.

Claims (2 — 0 Independent, 2 Dependent)

  1. Claim 2Depends on #1

    The method of preparing boron suboxide as claimed in claim 1, wherein the admixture consists essentially of a stoichiometric ratio of boron and zinc oxide.

  2. Claim 3Depends on #1

    The method of preparing boron suboxide as claimed in claim 1, wherein the step of subjecting the volume to an inert atmosphere is provided by a stream of inert gas movable through said volume, and wherein the gaseous metallic zinc is contacted by the inert gas and removed from said volume.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.

Non-Patent Literature (1)

  • Searcy et al., Journal of Physical Chemistry, Vol. 61, July, 1957, pp. 757 960.