Patents
US 3,645,801 A#9731655 Most CitedExpiredUnited States (USPTO)Utility

Method of producing rolled steel having high-strength and low-impact transition temperature

10Forward Citations (#9731655 Global)
0.2/yrCitation Velocity (#34452054 Global)
14.45Citation PageRank (#574990 Global)
4Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Rolled steels characterized in their as-rolled condition by an unexpected combination of high-strength and low-impact transition temperature. The product is produced by rolling a steel workpiece containing both austenite and ferrite, preventing complete recrystallization at any time thereafter, and continuing the rolling of said workpiece as it is cooling in the temperature range between the Ar1 temperature and 600* F.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 10.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 2Independent Claim

    Method of rolling a steel workpiece containing not more than 0.35 percent carbon and not more than a total of 3 percent of other elements other than iron comprising: a. rolling said workpiece in one or more passes as it is cooling from a temperature at which it is austenitic but while its temperature is still above the Ar3 temperature, b. continuing the rolling of said workpiece in one or more passes including at least one reduction pass as it is cooling in the temperature range between the Ar3 and the Ar1 temperatures, c. continuing the rolling of said workpiece in one or more passes includin

  2. Claim 3Independent Claim

    Method

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗