Patents
US 3,635,751 A#2334064 Most CitedExpiredUnited States (USPTO)Utility

Lithium silicate glare-reducing coating and method of fabrication on a glass surface

29Forward Citations (#2334064 Global)
0.5/yrCitation Velocity (#14678362 Global)
12.83Citation PageRank (#701413 Global)
4Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A novel optical screen comprises, as its viewing surface, a hard, abrasion-resistant coating having a rough, glare-reducing surface and composed of a lithium silicate material. The screen may be prepared by a novel method comprising: (a) warming the surface of a glass support to about 30* to 100* C., (b) coating the warm surface with an aqueous solution containing about 1 to 10 weight percent of a lithium-stabilized silica sol, (c) drying the coating, and then (d) heating the dry coating at about 150* C. to 450* C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 29.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 2Depends on #1

    The screen defined in claim 1 wherein said lithium silicate has an Si02:Li20 ratio of about 4:1 to 25:1.

  2. Claim 3Depends on #2

    A cathode-ray tube having a faceplate comprising the viewing screen defined in claim 2.

  3. Claim 4Independent Claim

    In a method for preparing an optical viewing screen having a glare-reducing viewing surface, the steps including a. warming the surface of a glass support to about 30* C. to 100* C., b. coating said surface with an aqueous solution containing about 1 to 10 weight percent of a lithium-stabilized silica sol, said sol having an Si02:Li20 ratio of about 4:1 to 25:1, c. drying said coating, d. and then heating said dry coating at about 100* C. to 450* C. for about 10 to 60 minutes.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗