Patents
US 3,615,902 A#5602999 Most CitedExpiredUnited States (USPTO)Utility

Corrosion-resistant steel

16Forward Citations (#5602999 Global)
0.3/yrCitation Velocity (#25927980 Global)
4.22Citation PageRank (#4371954 Global)
0Prior Art Cited
3Claims (0 Indep. · 3 Dep.)
0Drawings / Sheets

Abstract

A method of producing a ductile, corrosion resistant steel sheet or foil by depositing a coating of chromium, copper, nickel and/or titanium onto the surface of about an 0.080-inch thick hot rolled pickled steel strip prior to any cold rolling, and then cold rolling the coated steel strip to tinplate or foil gauge. The coated steel may then be annealed at a temperature below the Ac1 temperature to completely recrystallize the steel without causing substantial alloying of the steel and coating metal.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 16.

Claims (3 — 0 Independent, 3 Dependent)

  1. Claim 2Depends on #1

    A method according to claim 1 in which said coating is vacuum deposited at a thickness of from 0.001 to 0.005 inch.

  2. Claim 3Depends on #1

    A method according to claim 1 in which the annealing step comprises box annealing at a temperature within the range of about 1,050* to about 1,300* F. for a time of from 1 to 5 hours.

  3. Claim 4Depends on #1

    A method according to claim 1 in which the annealing step comprises a continuous anneal at a temperature within the range of about 1,050* to 1,300* F. for a period of less than one minute.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.