Method of activating impregnated catalyst
Abstract
Composites formed by the impregnation of refractory oxide supports with thermally decomposable salts of catalytically active metals are activated to produce highly active catalysts by heating the composites at a controlled rate to the prescribed calcination temperature while intimately contacting the composites with at least about 1 and preferably at least about 2 s.c.f.m. of injected air per pound of composite having an initial temperature below about 500* F.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 18.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
The method of claim 1 wherein said composite comprises at least about 1 weight percent of at least one compound of at least one metal selected from Groups VI and VIII of the Periodic Chart convertible to the corresponding metal oxide upon exposure to said oxidizing gas at said calcination temperature.
- Claim 3Depends on #1
The method of claim 1 wherein said composite is formed on impregnation of a foraminous support with a catalytic amount of at least one thermally decomposable water-soluble compound of the Group VI and VIII metals, convertible to the corresponding metal oxide upon exposure to said oxidizing gas at said calcination temperature, and said composite is heated to said calcination temperature at a rate of less than about 400* F. per hour.
- Claim 4Depends on #1
The method of claim 1 wherein said composite is formed by impregnation of a foraminous support with the aqueous
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗