A hydrated alumina which has been calcined to reduce its loss on ignition to below 12 percent and which is capable of at least partial rehydration is mixed with water and a blowing agent to form a slurry. The slurry is heated to below 100* C. to activate the blowing agent causing bubbles to form in the slurry. The slurry is then poured into a mold and heated to cause the alumina to rehydrate stabilizing the foamed body which is then activated at 350*-700* C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 12.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
The method of claim 1, wherein the finely divided alumina is admixed prior to partial rehydration with a portion of unground, selectively calcined alumina.
- Claim 3Depends on #1
The method of claim 1, wherein the curing temperature is of from 70* to about 95* C.
- Claim 4Depends on #1
The method of claim 1 wherein the amount of water added to the finely divided alumina is sufficient to produce a free-flowing slurry.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (12 of 12 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.