Removal of excess molten metal coatings by gas blast without ripple formations on coated surfaces
Abstract
An improvement in the method of controlling a metal material in a hot-dip metal plating process jetting at least one stream of compressed gas toward the metal plating coating on the surface of the sheet metal material drawn out of a hot-dip bath before said plating coating has solidified. The stream of compressed gas when it collides with the coated sheet metal material forms an upwardly flowing branch stream of gas. The improvement lies in directing at least one stream of ripple eliminating gas at a pressure at least substantially equal to the pressure of the first mentioned stream of compressed gas downwardly and toward the metal plating coating on the surface of the sheet material from a point above the point at which said first mentioned stream of gas is directed at the surface of the sheet material and at a point ahead of, with respect to the direction of advance of the sheet material, the point at which the metal plating coating solidifies and sufficiently close to the point at which the first mentioned stream of gas collides with said sheet material to cancel the upwardly flowing branch stream of gas. The stream of ripple eliminating gas prevents formation of ripple patterns
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 49.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
The improvement as claimed in claim 1 in which the stream of ripple eliminating gas is directed downwardly at an angle of from 45 to 60* to a normal to the surface of the sheet material, and has an elongated cross sectional shape extending in the direction of the width of the sheet material.
- Claim 3Depends on #1
The improvement as claimed in claim 1 in which the point at which the stream of ripple eliminating gas collides with the sheet material is spaced a distance of up to 10 mm. above the point at which the first mentioned stream of gas collides with said sheet material.
- Claim 4Depends on #3
The improvement as claimed in claim 3 in which the point at which the stream of ripple eliminating gas collides with the sheet material is spaced a distance of up to 2 mm. above the point at which the first mentioned stream of gas collides with said sheet material.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗