Process for the manufacture of filamentary carbon products
Abstract
Process for the manufacture of carbon and graphite filamentary products from polyacrylonitrile filamentary material wherein said filamentary material is subjected to a preliminary tension-free noncombustive partial oxidation and thereafter stretched to introduce or restore orientation in the polymer strands prior to being oxidized under tension followed by carbonization in a nonoxidizing atmosphere at a temperature of at least 700* C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 9.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 2Independent Claim
In a process for the manufacture of carbon and graphite filament and yarn which comprises subjecting a precursor polyacrylonitrile filamentary material (a) to a noncumbustive oxidation process consisting of a continuous phase carried out under tension and a secondary batch phase carried out without tension, and (b) to a carbonization stage in a nonoxidizing atmosphere at a temperature of at least 700* C., the improvement which consists in first subjecting the filamentary material to a preliminary substantially tension-free noncombustive partial oxIdation in air at a temperature within the rang
- Claim 3Depends on #1
The process of claim 1 wherein the entire se
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (9 of 9 total)
References Cited — Backward Prior Art (4)
Non-Patent Literature (1)
- Vosburgh Textile Research Journal Vol. 30, 1960, pages 882 896