Process for recovering sodium fluosilicate in the production of phosphoric acid

5Forward Citations (#19936127 Global)
0.1/yrCitation Velocity (#46618747 Global)
1.75Citation PageRank (#18051546 Global)
4Prior Art Cited
3Claims (0 Indep. · 3 Dep.)
0Drawings / Sheets

Abstract

A process for preparing sodium fluosilicate comprising treating mineral phosphates with an excess amount of aqueous sulfuric acid, removing excess sulfate from the resulting solution by precipitating the excess sulfate in the form of calcium sulfate by adding to the solution a stoichiometric quantity to said sulfate of phosphorites at a temperature of from 50* to 80* C., and then curing the precipitate at a temperature of from 20* to 40* C. for a period of time of from 1 to 5 hours, and then precipitating fluorine and silica from the solution in the form of sodium fluosilicate, after separating calcium sulfate therefrom, by adding monosodium phosphate, bisodium phosphate or a mixture thereof to the solution in a quantity such that the atomic ratio of the sodium contained in the mono- or bisodium phosphate to the fluorine contained in the solution is within the range of from 1:1 to 2.5:1, the precipitation being carried out at a temperature of from 40* to 100* C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 5.

Claims (3 — 0 Independent, 3 Dependent)

  1. Claim 2Depends on #1

    The method of claim 1 where the precipitated calcium sulfate which is removed from the solution is recycled to the solution prior to the calcium sulfate precipitation step in an amount of from 2 to 8 percent by weight of the solution, said calcium sulfate precipitation being carried out at a temperature of from 60* to 70* C.

  2. Claim 3Depends on #2

    The method of claim 2 wherein the calcium sulfate is recycled to the solution in a quantity of from 3 to 5 percent by weight of the solution.

  3. Claim 4Depends on #1

    The method of claim 1 wherein the solution to which the mono-or bisodium phosphates are added contains from 200 to 450 g./l. of phosphate as P2O5, up to 35 g./l. of fluoride as F , and up to 18 g./1. of silicate as SiO2.