Method of producing aluminum brazed coil
Abstract
A method of producing an all-aluminum coil is disclosed. In accordance with the method disclosed, hairpin coil tubes and coil fins are assembled with headers, return bends and inlet and outlet tubes. The ends of the hairpin tubes are expanded to receive the return tube portions with a predetermined clearance and the tubes are loaded with a solder ring at the expanded ends thereof. The fins are provided with solder-clad spacing collars around openings therethrough through which the hairpin tubes extend. The hairpin tubes are then expanded to mechanically secure the fin collars to the hairpin tubes. The assembled coil is then placed in a preheat oven and preheated to approximately 1,000* F. to bring the solder to a buttery consistency, after which the preheated coil assembly is immersed in molten Barium chloride salt at approximately 1,100* F. so that the solder rings and cladding on the collars braze the tubes and fins together. The brazed coil assembly is then washed in a hot ammonia bath. Sodium fluoride and lithium chloride fluxes are added to the salt bath to prevent oxidation of the coil components and to control the melting point of the salt bath, respectively.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 16.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of producing an aluminum coil comprising aSsembling coil components with aluminum alloy solder, preheating the assembled coil to approximately 1,000* F. to bring the solder to a buttery state, dipping the preheated assembled coil in a molten salt bath comprising as its major component barium chloride and also including sodium fluoride and lithium chloride flux maintained at approximately 1,100* F. to braze the coil components together, and removing the brazed coil from the salt bath and immersing the coil in an ammonia bath to neutralize the effects of fluxes thereon.
- Claim 2Depends on #1
The method as set forth in claim 1, wherein the solder includes 13 percent to 15 percent silicon, 0.25 percent copper, 0.70 percent iron, 0.25 percent zinc, 0.10 percent magnesium, 0.15 percent manganese and the balance aluminum.
- Claim 3Depends on #1
The method as set forth in claim 1, w
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 16 total)
References Cited — Backward Prior Art (7)
Non-Patent Literature (2)
- Brazing Manual, Published by American Welding Society, copyright 1963, pp.130 139
- Welding Handbook, Section 4, 5th Edition, published 1966, pp. 69.116 69.120.