Biaxially stretched trioxane copolymer film and process for the preparation thereof
Abstract
THE INVENTION RELATES TO A BIAXIALLY STRETCHED FILM AND PROCESS FOR THE PREPARATION THEREOF, THE FILM BEING A HIGH MOLECULAR WEIGHT LINEAR TRIOXANE/ETHYLENE OXIDE COPOLYMER HAVING STABILIZED END GROUPS AND CONTAINING 80 TO 99.9 PERCENT BY WEIGHT OF TRIOXANE BASED ON THE TOTAL WEIGHT OF THE POLYMER, THE FILM EXHIBITING A SAG OF LESS THAN 0.2 PERCENT CHARACTERISTIC FOR A FLAT FILM, A DEVIATION IN THICKNESS OF LESS THAN $6 PERCENT FROM THE AVERAGE THICKNESS, AN ELASTIC MODULUS IN ALL DIRECTIONS OF THE FILM PLANE OF AT LEAST 300 KG./MM.2, AN ULTIMATE TENSILE STRENGTH ABOVE 15 KG./MM.2 AT AN ELONGATION AT RUPTURE OF LESS THAN 100 PERCENT, AND A SHRINKAGE CAPACITY, AT 140*C., OF LESS THAN 5 PERCENT.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 2.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2002185774 A1 | Film-stretching system | — | 1 |
| US 4,569,983 A | Polymer materials | 1986 | 3 |
References Cited — Backward Prior Art (0)
No backward patent references recorded.