Abstract
A method for preserving the mechanical properties of steel wire or rod during spot welding of such steel wire or rod to form cages for use in prestressed concrete. The steel reinforcing rods are heated to a temperature of from 300-450* C. for from 5 seconds to 15 minutes after being spot welded.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 4.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of preventing deterioration of the mechanical properties of the welded parts of steel reinforcing rods due to spot welding during the formation of steel wire cages for manufacturing prestressed concrete structures, comprising heating the welded parts of said rods to a temperature of from about 300* to about 430* C. for about 5 to about 20 seconds after the spot welding is completed.
- Claim 2Depends on #1
A method as claimed in claim 1 in which said welded parts are heated to a temperature of from 420* to 430* C.
- Claim 3Depends on #1
A method as claimed in claim 1 in which said welded parts are heated to a temperature of from 300* to about 430* C. for 20 seconds.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (3)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 1,298,590 A | Electric-arc welding. | 1919 | 25 |
| US 2,314,691 A | Welding apparatus | 1943 | 17 |
| US 3,015,018 A | Heating apparatus | 1961 | 12 |