US 3,556,772 A#12724292 Most CitedExpiredUnited States (USPTO)Utility
Method of sponge iron briquetting
8Forward Citations (#12724292 Global)
0.1/yrCitation Velocity (#38296485 Global)
2.46Citation PageRank (#10457602 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets
Abstract
SPONGE IRON IS BRIQUETTED AT TEMPERATURES FROM 400 TO 800*C. AND PRESSURES FROM 1,500 TO 3,000 KG./CM.2 TO FORM BRIGUETTES HAVING A BULK DENSITY OF ABOUT 5G./CM.3. THESE BRIQUETTES ARE HEAVY ENOUGH TO SINK THROUGH THE SLAG IN A FURNACE AND DOWN INTO THE MOLTEN STEEL.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 8.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.