Process for the manufacture of polypropylene films
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 40.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A PROCESS FOR THE MANUFACTURE OF SHRINKABLE POLYPROPYLENE FILMS WHICH COMPRISES EXTRUDING PREDOMINATELY ISOTACTIC POLYPROPYLENE AT A TEMPERATURE IN THE RANGE OF ABOUT 190 TO 325*C. THROUGH A SHEET DIE HAVING A WIDTH SUCH AS TO GIVE THE RESULSTING FILM A THICKNESS GREATER THAN 0.3 MM., QUENCHING THE EXTRUDED MELT AT A TEMPERATURE BELOW 90%C., PRE-HEATING THE FILM FOR LONGITUDINAL STRETCHING TOA TEMPERATURE IN THE RANGE OF (TI-5* C.) TO T1 (T1=130 TO 140*C.), FURTHER HEATING THE FILM IN CONTACT WITH A ROLL MAINTAINED AT A TEMPERATURE T2 (T2=140 TO 150*C.), STRETCHING THE FILM TO 5 TO 7 TIMES ITS
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗