Preparation of dense uranium oxide
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 8.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A METHOD OF PRODUCING A DENSE URANIUM OXIDE BODY WHICH COMPRISES COMPACTING AN URANIUM OXIDE POWDER HAVING A SURFACE AREA PER UNIT WEIGHT OF FROM 1 TO 18 SQ. METRES/GM. HEATING THE COMPACTED BODY IN A STEAM-CONTAINING ATMOSPHERE TO SINTERING TEMPERATURES, SINTERING THE COMPACTED BODY IN A STEAM ATMOSPHERE BELOW ABOUT 1450*C., AND SUBJECTING THE SINTERED BODY WHILE ABOVE ABOUT 1000*C. TO A HYDROCARBONACEOUS REDUCING GAS CONTAINING HYDROGEN IN AMOUNTS FROM ABOUT 3 TO 25 VOLUME PERCENT UNTIL THE O/U RATIO IS REDUCED TO BELOW ABOUT 2.025.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 3,051,566 A | Process for producing high density refractory bodies | 1962 | 42 |
| US 3,087,876 A | Method of sintering uranium dioxide | 1963 | 5 |