Coalescence process using polyolefin fiber
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 8.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A PROCESS FOR THE COALESCENCE OF A HAZY HYDROCARBON OIL COMPRISING WATER DISPERSED IN KEROSENE WHICH COMPRISES PASSING SAID OIL THROUGH A LAYER FROM ABOUT 20 TO ABOUT 50 CENTIMETERS THICK OF POLYPROPYLENE FIBERS HAVING A FIBER DIAMETER OF FROM ABOUT 3 TO ABOUT 100 MICRONS, HAVING A FIBER LENGTH AT LEAST ABOUT 100 TIMES THE FIBER DIAMETER, WHEREIN SAID POLYPROPYLENE HAS A MOLECULAR WEIGHT OF FROM ABOUT 100,000 TO ABOUT 300,000, WHEREIN THE FREE SPACE OF THE LAYER IS FROM ABOUT 88 TO ABOUT 95%, AND WHEREIN SAID OIL IS PASSED THROUGH THE LAYER AT A SUPERFICIAL VELOCITY OF FROM ABOUT 0.5 TO ABOUT