Agglomeration of bauxite fines
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 6.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A METHOD FOR AGGLOMERATING BAUXITE FINES WHICH COMPRISES: MIXING BAUXITE FINES WHICH HAVE BEEN CALCINED AT A TEMPERATURE WITHIN THE RANGE OF ABOUT 600*F. TO ABOUT 1600*F. TO A BOLATILE MATTER CONTENT BELOW 10% WITH A SUFFICIENT QUANTITY OF A MIXTURE OF SULFURIC ACID AND PHOSPHORIC ACID TO PERMIT AGGLOMERATION OF SAID FINES, SAID MIXTURE OF ACIDS BEING OF 90% TO 100% CONCENTRATION AND CONTAINING FROM ABUT 1 1/2 TO ABOUT 3 1/2 PARTS BY WEIGH TOF ''ISO4 TO 1 PART BY WEIGHT OF H3PO4, FORMING THE MIXTURE INTO AGGLOMERATES, HEATING SAID AGGLOMERATES AT A TEMPERATURE WITHIN THE RANGE OF ABOUT
Technical Overview & Description