Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 26.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A METHOD FOR CONVERTING A POLYMER SELECTED FROM THE GROUP CONSISTING OF HOMOPOLYMERS OF ALIPHATIC MONO1-OLEFINS HAVING FROM 2 TO 8 CARBON ATOMS PER MOLECULE AND COPOLYMERS OF MIXTURES OF ALIPHATIC MONO-1-OLEFINS HAVING FROM 2 TO 8 CARBON ATOMS PER MOLECULE INTO A MATERIAL HAVING A FINELY DIVIDED FORM WHICH COMPRISES SUBJECTING A MIXTURE OF SAID POLYMER WITH A CHEMICAL BLOWING AGENT TO A TEMPERATURE IN THE RANGE OF ABOUT 250*F. TO ABOUT 500*F. AT A PRESSURE IN THE RANGE OF ATMOSPHERIC TO 800 P.S.I.G., THE AMOUNT OF SAID CHEMICAL BLOWING AGENT BEING THE RANGE OF ABOUT 1 TO ABOUT 40 PARTS BY WEIG