Hydrophobic organophilic particulate matter
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 22.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
THE METHOD OF TREATING HYDROPHILIC PARTICULATE MATERIAL TO PROVIDE A HYDROPHOBIC ORGANOPHILIC PARTICULATE MATERIAL COMPRISING THE STEPS OF FORMING ANAQUEOUS SLURRY OF SAID PARTICULATE MATERIAL, ADDING TO SAID SLURRY ABOUT 0.25% TO 1% OF ETHYLENE DIAMINE, ADDING TO THE DIAMINE TREATED MATERIAL ABOUT 75% OF THE AMOUNT OF AN OLEIC ACID WHICH WILL PRIDUCE THE "OPTIMUM LEVEL OF VISCOSITY" IN MINERAL OIL, ADJUSTING THE PH TO ABOUT PH 3 TO PH 5 WITH ALUMINUM SULFATE, READJUSTING TO ABOUT PH 6.5 TO PH 7.5 WITH AMMONIUM HYDROXIDE, SEPARATING THE PARTICULATE MATERIAL FROM THE AQUEOUS PHASE AND D
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 22 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2,852,406 A | Pigment composition and process for its production | 1958 | 15 |
| US 2,982,665 A | Modified kaolin clay | 1961 | 39 |