Selective removal of excess solder
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 18.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
THE METHOD OF REMOVING EXCESS TIN-LEAD SOLDER PROJECTING BEYOND A DESIRED PLANE SPACED FROM ONE SURFACE OF A PRINTED CIRCUIT BOARD ON WHICH THE SOLDER IS DEPOSITED AND FROM WHICH EXCESS SOLDER IS TO REMOVED, THE DESIRED PLANE BEING LOCATED AT THE SAME SIDE OF THE CIRCUIT BOARD AS SAID ONE SURFACE, COMPRISING THE STEPS OF SKIMMING SAID ONE SURFACE OF THE CIRCUIT BOARD ABOVE THE SURFACE OF A LIQUID BATH OF LOW-MELTING QUATERNARY ALLOY OF BISMUTH, LEAD, TIN AND CADMIUM HEATED TO A TEMPERATRURE OF ABOUT 200*F., THE LOW-MELTING ALLOY COMPRISING BETWEEN 48% AND 55% OF BISMUTH, LESS THAN 33% LEAD, AN