Extrusion-devolatilization process

9Forward Citations (#11169316 Global)
0.1/yrCitation Velocity (#38276064 Global)
2.85Citation PageRank (#8238365 Global)
10Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 9.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A METHOD OF IMPROVING THE HEAT RESISTANCE AND LIGHT STABILITY OF COPOLYMERS OF ALPHA-ALKYL STYRENES AND ALKYL METHACRYLATES WHICH COMPRISES PASSING A CRUDE COPOLYMERIC MASS COMPRISING 15 TO 40 PARTS BY WEIGHT OF AN ALPHA-ALKYL STYRENE AND 60 TO 85 PARTS BY WEIGHT OF AN ALKYL METHACRYLATE, EACH OF THE SAID ALKYL GROUPS HAVING FROM 1 TO 4 CARBON ATOMS, AND UNREACTED MONOMERS THROUGH A SCREW EXTRUDER AT A TEMPERATURE WITHIN THE RANGE OF 400* TO 530*F. AND A VACUUM OF 2 TO 100 MM. OF MERCURY ABSOLUTE PRESSURE FOR A PERIOD OF TEME SUFFICIENT TO VOLATILIZE MONOMERIC MATERIALS CONTAINED THEREIN AND R