Heat hardenable chromium-nickel-aluminum steel
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 16.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A CHROMIUM-NICKEL-ALUMINUM STEEL WHICH IS SUBSTANTIALLY FULLY AUSTENITRIC AT ANNEALING TEMPERATURES AND WHICH IS HARDENABLE BY HEAT-TREATMENT, SAID STEEL CONSISTING ESSENTIALLY OF ABOUT: 4% TO 14.5% CHROMIUM, 6% TO 12% NICKEL, .5% TO 2% ALUMINUM, 4% TO 14% MOLYBDENUM, MANGANESE UP TO 2%, SILICON UP TO 1%, CARBON UP TO .20%, UP TO ABOUT 0.10% OF THE GROUP CONSISTING OF TITANIUM AND ZIRCONIUM, UP TO ABOUT 0.50% COLUMBIUM, BORON UP TO 0.010%, AND REMAINDER SUBSTANTIALLY ALL IRON, WITH ADDITIONAL MANGANESE, IN EXCESS OF SAID 2%, PARTIALLY SUBSTITUTED FOR SAID NICKEL ON THE BASIS OF 2 FOR 1, THE AC
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 16 total)
References Cited — Backward Prior Art (5)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2,505,763 A | Stainless steel and method | 1950 | 10 |
| US 2,506,558 A | Stainless steel and method | 1950 | 10 |
| US 2,590,835 A | Alloy steels | 1952 | 37 |
| US 2,958,617 A | Method for hardening chromiumnickel stainless steel | 1960 | 9 |
| US 2,999,039 A | Martensitic steel | 1961 | 21 |