Method for repair of defective pump casings
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 5.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
METHOD OF REPAIRING THE DEFECTIVE INTERIOR SHROUD SURFACE OF A PUMP CASING COMPRISING THE STEPS OF: MOUNTING THE PUMP CASING FOR ROTATION IN A SUBSTANTIALLY VERTICAL PLANE; PLACING THE BOTTOM OF THE CASING IN A SAND BASE TO PREVENT BURN THROUGHS AND PREHEATING THE CASING, INTRODUCING A PREDETERMINED CHARGE OF REACTED THERMIT METAL INTO THE BOTTOM INTERIOR PORTION OF THE CASING; ROTATING THE PUMP CASING WHILE IN SAID BASE TO CONSECUTIVE ANGULARLY DISPLACED POSITIONS IN THE VERTICAL PLANE AND INTRODUCING ADDITIONAL CHARGES OF THERMIT METAL INTO THE BOTTOM OF THE CASING AT EACH OF THE ANGULARLY D
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (5 of 5 total)
References Cited — Backward Prior Art (5)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 1,355,224 A | Chemical welding | 1920 | 12 |
| US 1,831,301 A | Brake releasing device | 1931 | 4 |
| US 1,920,022 A | Bearing manufcture | 1933 | 6 |
| US 1,934,901 A | Process for producing metal rollers | 1933 | 5 |
| US 2,358,090 A | Process of bonding metals | 1944 | 16 |