Zirconium-aluminum-phosphorus catalyst and method for preparing the same, employed for the cracking of hydrocarbons

22Forward Citations (#3548475 Global)
0.3/yrCitation Velocity (#22238371 Global)
11.39Citation PageRank (#855532 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 22.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 7Independent Claim

    A METHOD FOR CRACKING A HYDROCARBON CHARGE WHICH COMPRISES CONTACTING THE SAME UNDER CATALYTIC CRACKING CONDITIONS WITH A CATALYST CONSISTING ESSENTIALLY OF AN OXYGEN-CONTAINING COMBINATION OF ALUMINUM, ZIRCONIUM AND PHOSPHORUS WHEREIN THE ATOMIC RATIO OF ALUMINUM TO ZIRCONIUM IS BETWEEN ABOUT 0.1 AND ABOUT 10 AND IN WHICH THE ATOMIC RATIO OF THE COMBINED ALUMINUM AND ZIRCONIUM CONTENT TO PHOSPHORUS IS BETWEEN ABOUT 0.1 AND ABOUT 10, SAID CATALYST RESULTING FROM REACTION, IN AQUEOUS SOLUTION, OF A WATER-SOLUBLE SALT OF ALUMINUM, A WATER-SOLUBLE SALT OF ZIRCONIUM AND A WATER-SOLUBLE COMPOUND SE