Method for improving the extrudability of crystalline polyolefins with aliphatic alcohols
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 17.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A METHOD FOR IMPROVING THE EXTRUDABILITY OF A HIGHLY CRYSTALLINE POLYMER OF A 1-OLEFIN, SAID POLYMER HAVING A DENSITY OF AT LEAST 0.94 AT 20*C., COMPRISING ADDING TO THE POLYMER A MINOR AMOUNT OF AN ALIPHATIC ALCHOL CONTAINING OXYGEN ONLY IN HYDROXYL GROUPS AND CONTAINING 10 TO 25 CARBON ATOMS PER MOLECULE.
- Claim 10Independent Claim
IN THE POLYMERIZATION PROCESS COMPRISING CONTACTING A MEMBER SELECTED FROM THE GROUP CONSISTING OF ETHYLENE AND MIXTURES OF ETHYLENE WITH OTHER 1-OLEFINS WITH A SUSPENSION OF A CHROMIUM OXIDE:CONTAINING CATALYST IN A LIQUID HYDROCARON AT A TEMPERATURE SUCH THAT SUBSTANTIALLY ALL OF THE POLYMER PRODUCED IS INSOLUBLE IN SAID LIQUID HYDROCARBON AND IS DIFFICULTY EXTRUDABLE, THE IMPROVEMENT COMPRISING ADDING TO THE POLYMER A MINOR AMOUNT OF AN ALIPHATIC ALCOHOL CONTAINING OXYGEN ONLY IN HYDROXYL GROUPS AND CONTAINING 10 TO 25 CARBON ATOMS PER MOLECULE, SAID ALIP
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗