Process of reacting polyethylene-butyl rubber blend with dicumyl peroxide and n-methyl-n-nitroso-4-nitrosoaniline
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 6.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A PROCESS FOR PREPARING A MODIFIED BLEND OF POLYETHYLENE AND BUTYL RUBBER COMPRISING REACTING 100 PARTS BY WEIGHT OF POLYETHYLENE HAVING A MOLECULAR WEIGHT IN THE RANGE OF 12,000 TO 500,000; 5 TO 50 PARTS BY WEIGHT OF BUTYL RUBBER WHICH IS A COPOLYMER OF ABOUT 90 TO 99.5% ISOBUTYLENE AND ABOUT 10 TO 0.5% OF A CONJUGATED DIOLEFIN; 0.3 TO 0.7 PART BY WEIGHT OF DICUMYL PEROXIDE; 0.5 TO 1 PART BY WEIGHT OF N-METHYL-N-NITROSO-4-NITROSOANILINE AT A TEMPERATURE IN THE RANGE OF 275 TO 290* F. FOR A TIME IN THE RANGE OF 8 TO 12 MINUTES TO PRODUCE SAID MODIFIED BLEND.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗