Patents
US 2,958,618 A#7167961 Most CitedExpiredUnited States (USPTO)Utility

Method for hardening chromiumnickel stainless steel

13Forward Citations (#7167961 Global)
0.2/yrCitation Velocity (#32507570 Global)
13.05Citation PageRank (#682020 Global)
2Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 13.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    IN THE PRODUCTION OF HEAT-HARDENED CHROMIUMNICKEL STAINLESS STEEL PRODUCTS, THE ART WHICH COMPRISES ANNEALING A HEAT-HARDENABLE CHROMIUM-NICKEL STAINLESS STEEL AT A TEMPERATURE OF 1900* TO 2050*F., FORMING THE STEEL INTO PRODUCTS OF DESIRED CONFIGURATION, CONDITIONING THE SAME AT A TEMPERATURE OF 1000* TO 1200*F. FOR PERIODS OF TIME RANGING FROM ABOUT 3 MINUTES AT THE 1200* F. TEMPERATURE UP TO ABOUT 48 HOURS AT THE TEMPERATURE OF 1000*F., REFRIGERATING THE PRODUCTS AT A TEMPERTURE OF ABOUT -30* TO -150*F, AND REHEATING THE PRODUCTS AT A TEMPERATURE OF ABOUT 700* TO 1150*F. TO HARDEN THE SAME.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (2)