Process for preventing the formation of voids and pock marks in the extrusion of olefin polymers
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 6.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 8Independent Claim
IN THE PROCESS OF EXTRUDING 1-OLEFIN POLYMERS AS STRANDS, THE IMPROVEMENT COMPRISING PASSING THE EXTRUDED STRAND THROUGH A FIRST FLUID HAVING A TEMPERATURE IN THE RANGE 40 TO 150*F. FOR A TIME TO HARDEN ONLY THE SURFACE OF SAID STRAND, PASSING THE STRAND THROUGH A SECOND FLUID WHEREIN THE HEAT OF SAID STRAND IS REDISTRIBUTED THEREBY SOFTENING SAID SURFACE AND THEREAFTER PASSING SAID STRAND THROUGH A THIRD FLUID HAVING A TEMPERATURE OF AT LEAST 150*F. AND AT LEAST 20*F. ABOVE SAID FIRST FLUID AND BELOW THE SOFTENING POINT OF THE POLYMERS FOR A TIME SUFFICIENT TO HARDEN THE ENTIRE STRAND.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗