Electrically conductive glass composition containing suboxides of titanium and method of making the same
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 21.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 10Independent Claim
THE METHOD OF PREPARING AN ELECTRICALLY CONDUCTIVE GLASS COMPOSITION, SAID METHOD COMPRISING THE STEPS, OF HEATING TOGETHER AT A TEMPERATURE SUBSTANTIALLY WITHIN THE RANGE OF 1300* AND 300*F. A COMMINUTED DRY MIXTURE OF AN ALKALI METAL OXIDE IN AN AMOUNT WITHIN THE RANGE OF 10-30% BY WEIGHT OF SAID COMPOSITION, SILICON DIOXIDE IN AN AMOUNT FROM 31-58% BY WEIGHT OF SAID COMPOSITION, FROM 14% TO 45% BY WEIGHT OF AN OXIDE OF TITANIUM SELECTED FROM THE GROUP CONSISTING OF TIO, TI2O3, TI3O5, AND MIXTURES THEREOF, AND THE ADDITIONAL COMPONENTS BEING CHOSEN FROM THE GROUP CONSISTING OF THE FOLLOWING
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 21 total)
References Cited — Backward Prior Art (4)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2,289,211 A | Titanium oxide composition | 1942 | 14 |
| US 2,497,235 A | ph-responsive glass electrodes | 1950 | 18 |
| US 2,587,916 A | Heat detecting cable | 1952 | 36 |
| US 2,786,819 A | Resistor | 1957 | 21 |