Method of making and drying shell-type refractory molds
Abstract
879,388. Making shell moulds. MELLEN, E. J. May 29, 1959 [June 17, 1958], No. 18433/59. Class 87(2). A refractory mould for casting metal is made by dipping a destructible pattern of e.g. wax, polystyrene or acrylic or methacrylic resins in a slurry, removing the pattern from the slurry and drying it in an air stream which has .a wet bulb temperature of room temperature and a dry bulb temperature not less than 5‹F. above room temperature, and then after drying, repeating the process until several layers have been built up. Successive coats may be dried at increased dry bulb temperatures e.g. 5‹F. per layer. The layers (except the last) may be dusted with refractory particles, e.g. silicon oxide glass. The slurry may be made from quartz, alumina, silicon carbide, graphite, aluminium silicate, flint, zirconium silicate, and silicon oxide glass, with colloidal silica or ethyl silicate as a binder, methyl cellulose as a thickener, and water or alcohol.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 35.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
THE METHOD OF PREPARING REFRACTORY MOLDS HAVING A WALL THICKNESS OF LESS THAN ONE-HALF INCH FOR CASTING METALS THEREIN COMPRISING THE STEPS OF (1) DIPPING A DESTRUCTIBLE PATTERN IN AN AQUEOUS SLURRY CONTAINING REFRACTORY MATERIALS AND A BINDER THEREFOR TO FORM A FIRST COATING OF REFRACTORY MATERIALS ON SAID PATERN, SAID PATTERN AND SAID SLURRY BEING AT ABOUT ROOM TEMPERATURE, (2) ADIBATICALLY DRYING SAID FIRST COATING SO THAT THE TEMPERATURE OF THE PATTERN REMAINS SUBSTANTIALLY CONSTANT, SAID DRYING BEING ACHIEVED BY THE USE OF A VOLUME OF AIR OF CONTROLLED HUMIDITY THAT IS MOVED RAPIDLY PAST
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗