Spinning nonfused glass fibers from an aqueous dispersion
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 34.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 3Independent Claim
THE METHOD OF PREPARING A GLASS FIBER AT ROOM TEMPERATUE FROM A STABLE HETEROGENOUS AQUEOUS SYRUP WHICH INCLUDES THE STEPS OF MIXING AT ROOM TEMPERATURE A DISPERSION OF GLASS-FORMING METAL OXIDES HAVING A PARTICLE SIZE WITHIN THE RANGE FROM 5 TO 140 MICRONS WITH A DISPERSION OF COLLOIDAL SILICA HAVING A PARTICLE SIZE LESS THAN 1 MICRON, ADDING TO THE RESULTING MIXTURE LESS THAN 2% BY WEIGHT BASED ON THE METAL OXIDE PARTICLES OF TRANSFORMING AGENT COMPRISING ABOUT 3.2% RUBBER FROM LATEX, ABOUT 1.3% ACRYLATE AND VINYL MATERIAL COMPRISING POLYVINYL ALCOHOL, POLYVINYL ACETATE, POLYMETHACRYLIC ACID
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 34 total)
References Cited — Backward Prior Art (3)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2,133,236 A | Glass wool and method and apparatus for making same | 1938 | 19 |
| GB 512,292 A | Process for the manufacture of glass | — | 3 |
| US RE24060 E | G russell | 1955 | 7 |