Process for heat-treating a bearing alloy
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 0.
Claims (1)
- Claim 1Independent Claim
A METHOD OF PRODUCING AN ALUMINIUM-ZINC-COPPER ALLOY FOR BEARING PURPOSES COMPRISING THE STEPS OF: PRODUCING A COMPOSITION ALLOY OF 35 TO 50% AL, 5.8 TO 8.3% CU, 0 TO 0.3% FE, 0 TO 0.25% SI, AND 59.2 TO 41.15% OF ZN; OF SHAPING SAID ALOY, AND OF HEAT-TREATING SAID ALLOY AT TEMPERATURE FROM 100 TO 280*C. FOR A TIME FROM 24 TO 48 HOURS.
Technical Overview & Description
PROCESS FOR HEAT-TREATING A BEARING ALLOY Erich Pelzel, Stolberg, Germany, assignor to Vereinigte Osterreichische Eiseuund Stahlwerke Aktiengesellscbaft, Linz (Danube), Austria, :1 firm No Drawing. Application July 5, 1956 Serial No. 595,835 Claims priority, application Austria February 9, 1952 2 Claims. (Cl. 148-13) The invention relates to an aluminum-zinc-copper alloy, which is particularly suitable for replacing the expensive bronzes containing copper and Zinc which have previously been used in most cases as a bearing alloy. The invention relates also to a process for heat-treating the bearing members made of that alloy. The present application is a continuation-in-part of the copending US. patent application Ser. No. 334,973 filed.February 3, 1953, now abandoned. 7 Many alloys are known which consist of aluminum and copper, balance zinc. Previously, however, such alloys have been used only in single cases in bearings. For this purpose not only the generally desired higher characteristics as regards tensile strength, elongation and Brinell hardness are to be taken into consideration but also the internal structure and the adherence of oil films on the bearing surface. In that respect too bronzes are preferable to alloys of zinc, aluminum and copper. In the co-pending application mentioned hereinbefore, an alloy was proposed for bearing purposes which contains 30-66% of aluminum, copper to the amount of at least one sixth and at most one fourth of the actual aluminum content, and the balance of zinc. The general technological properties of such alloys are satisfactory but it has been found in experiments that in certain marginal regions of the aluminum content disadvantages occur which cannot be tolerated where the alloy is used for bearing bushings. It has been found that the disintegration of the structure and resultant changes in volume increase as the content of aluminum is reduced. For instance, in an alloy consisting of 30% aluminum,
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (3)
| Patent | Title | Year | Citations |
|---|