Method of incorporating titanium into selectively transparent silica glass

9Forward Citations (#10976362 Global)
0.1/yrCitation Velocity (#40818992 Global)
4.55Citation PageRank (#3868083 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 9.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    IN THE PREPARATION OF SELECTIVELY TRANSPARENT SILICA GLASS BY HEATING TO ABOUT 1750* C. AND THEN COOLING A MIXTURE CONSISTING OF SUBSTANTIALLY PURE SILICON DIOXIDE AND TITANIUM DIOXIDE IN AN AMOUNT EFFECTIVE TO RENDER THE GLASS SUBSTANTIALLY OPAQUE TO LIGHT RADIATION OF 1850 A.U. WHILE BEING TRANSPARENT TO RADIATION OF 2537 A.U., THE METHOD OF INCORPORATING THE TITANIUM INTO THE SILICON DIOXIDE PRIOR TO HEATING COMPRISING MIXTING AN AQUEOUS SOLUTION OF A WATER-SOLUBLE TITANIUM SALT WITH A MASS OF SILICA PARTICLES IN AN AMOUNT TO SUBSTANTIALLY FILL THE VOIDS BETWEEN SAID PARTICLES, ADDING A BAS