US 2,860,079 A#87839976 Most CitedExpiredUnited States (USPTO)Utility

Heat treating process for a 2% fe 2% cr 2% mo titanium base alloy

0Forward Citations (#87839976 Global)
0.0/yrCitation Velocity (#87839976 Global)
0.56Citation PageRank (#87839976 Global)
2Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    THE PROCESS OF TREATING A TITANIUM ALLOY INCLUDING ABOUT 2% IRON, ABOUT 2% CHROMIUM AND ABOUT 2% MOLYBDENUM COMPRISING HEATING TO APPROXIMATELY 1650* F. TO FORM THE BATE PHASE, MAINTAINING THIS TEMPERATURE UNTIL SUCH TIME AS THE MATERIAL BECOMES STABILIZED, FURNACE COOLING TO 1325* F. AND MAINTAINING THIS TEMPERATURE FOR APPROXIMATELY 1O HOURS PERMITTING COARSE ALPHA PHASE IN EQUILIBRIUM WITH BETA PHASE TO FORM WITHOUT PERMITTING FINE ALPHA TO FORM, COOLING TO 1200* F. AND MAINTAINING THIS TEMPERATURE FOR 24 HOURSS TO PREVENT FINE ALPHA FROM FORMING, AND AIR COOLING TO ROOM TEMPERATURE.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (2)