Patents
US 2,848,360 A#53754111 Most CitedExpiredUnited States (USPTO)Utility

Method of treating nickel-beryllium alloys

1Forward Citations (#53754111 Global)
0.0/yrCitation Velocity (#61796101 Global)
0.82Citation PageRank (#53754111 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A METHOD OF TREATING A NICKEL BASE ALLOY HAVING INCLUDED THEREIN A METAL SELECTED FROM THE GROUP CONSISTING OF BERYLLIUM IN AN AMOUNT BETWEEN 2.5% AND 4.5%, BY WEIGHT, AND MAGNESIUM, IN AN AMOUNT BETWEEN 0.6% AND 2.0%, BY WEIGHT, IN ORDER TO GIVE TO SAID ALLOY A HIGH FACTOR OF REAL SECONDARY EMISSION, THE RELATIVE CONCENTRATION OF NICKEL BEING SUFFICIENT TO PROVIDE A SATURATED SOLID SOLUTION OF SAID METAL IN THE NICKEL; SAID METHOD COMPRISING THE STEPS OF WATER-QUENCHING THE ALLOY FROM A TEMPERATURE OF ABOUT 1100*C., COMPRESSING THE ALLOY AT A PRESSURE OF ABOUT 10 KG. PER SQ. CM. AND AT A TEMP

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)