High damping alloy and members prepared therefrom
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 15.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A MEMBER SUITABLE FOR USE AS A TURBINE BLADE, HAVING HIGH DAMPING PROPERTIES AT 1200*F., COMPRISING A MEMBER OF AN ALLOY COMPOSED OF, BY WEIGHT, FROM 65% TO 88% COBALT, FROM 1% TO 2% TITANIUM, FROM 0.1% TO 1.5% ALUMINUM, THE TOTAL OF TITANIUM, AND ALUMINUM BEING AT LEAST 1.5%, CARBON NOT EXCEEDING 0.05%, AND THE BALANCE, AT LEAST 8%, BEING NICKEL, WITH IMPURITIES NOT EXCEEDING 1%, THE WROUGHT BLADE HAVING BEEN SOLUTION TREATED ABOVE 1600*F. AND ABOVE THE RECRYSTALLIZATION TEMPERATURE OF THE ALLOY. AND THEN AGED AT FROM ABOUT 1200*F. TO 1400*F. FOR AT LEAST 4 HOURS TO PRECIPITATION HARDEN THE A
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 15 total)
References Cited — Backward Prior Art (3)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2,011,976 A | Cobalt-tungsten-iron alloy | 1935 | 3 |
| US 2,018,520 A | High strength alloy | 1935 | 7 |
| US 2,121,759 A | Alloy | 1938 | 4 |