Patents
US 2,824,818 A#10936030 Most CitedExpiredUnited States (USPTO)Utility

Welding of metals having hot-short characteristics

9Forward Citations (#10936030 Global)
0.1/yrCitation Velocity (#40802740 Global)
6.55Citation PageRank (#2133230 Global)
0Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 9.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A METHOD OF ARC WELDING METALS THAT HAVE THE CHARACTERISTIC OF BEING MORE BRITTLE AT ARC WELDING TEMPERATURES THAN AT NORMAL ROOM TEMPERATURE, COMPRISING THE STEPS OF PEENING THE EDGES TO BE WELDED AND AN AREA IMMEDIATELY ADJACENT TO SAID EDGES TO THE EXTENT NECESSARY TO PLACE COMPRESSION STRESSES IN THE METAL SUFFICIENT TO COMPENSATE FOR TENSILE STRESSES DEVELOPED DURING HEATING TO WELDING TEMPERATURE, COOLING SAID PEENED EDGES AND AREA TO A SUB-ZERO TEMPERATURE OF AT LEAST -40*F., ARC WELDING A SMALL INCREMENT OF WELD METAL BETWEEN SAID EDGES, REMOVING THE ACCUMULATED WELDING SLAG FROM THE D

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.

Non-Patent Literature (1)

  • None