Process of treating tin bronze
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 10.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
THE METHOD OF PRODUCING A DEOXIDIZED TIN BRONZE HAVING AN ENDURANCE STRENGTH EXCEEDING 40,000 POUNDS PER SQUARE INCH AT 10,000,000 CYCLES, WHICH COMPRISES SUBJECTING A BRONZE CONTAINING 1 1/2% TO 12% TIN, 0.001% TO 0.5% RESIDUAL DEOXIDIZER, AND THE BALANCE ESSENTIALLY ALL COPPER TO COLD WORKING AND THEN ANNEALING AT A TEMPERATURE IN THE RANGE FROM 500*C.TO 600*C. FOR A SUFFICIENT PERIOD OF TIME TO EFFECT SUBSTANTIALLY COMPLETE RECRYSTALLIZATION WITHOUT INCREASING THE AVERAGE GRAINS SIZE TO ABOVE 0.045 MM., THEN SUBJECTING THE BRONZE TO SEVERE COLD WORKING SUFFICIENT TO EFFECT A REDUCTION IN CR
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (10 of 10 total)
References Cited — Backward Prior Art (1)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2,676,123 A | Treatment of brass | 1954 | 17 |