Method of surface treating and extruding die with chromium
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 9.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
IN A METHOD OF SURFACE TREATING AN EXTRUDING DIE FORMED OF STEEL OF APPROXIMATELY 50 ROCKWELL C HARDNESS COMPRISING THE STEPS OF COATING SAID DIE WITH A LAYER OF CHROMIUM OF PREDETERMINED THICKNESS, HEATING SAID COATED DIE AT APPROXIMATELY 2800* F. FOR A PERIOD OF APPROXIMATELY SIX HOURS TO FORM AN AUSTENITIC CHROME STEEL LAYER RESULTING FROM PENETRATION OF THE STEEL BY THE CHROMIUM, AIR COOLING SAID HEATED DIE FOR APPROXIMATELY SIX HOURS TO STABILIZE THE AUSTENITIC LAYER FORMED ON THE SURFACE OF SAID DIE, REHEATING SAID DIE AT APPROXIMATELY 1800* F. TO OBTAIN A FINE GRAIN OF AUSTENETIC LAYER