Method of preparing zinc sulfide phosphor
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 9.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A PROCESS FOR THE PRODUCTION OF A PHOSPHORESCENT ZINC SULPHIDE WHICH COMPRISES THE STEPS OF MIXING ZINC OXIDE AND SULPHUR IN A PROPORTION TO FORM ZINC SULPHIDE WITH AN EXCESS OF SULPHUR, HEATING THE MIXTURE WITH AN ALKALI HALIDE TO APPROXIMATELY 800* C., MAINTAINING THE MIXTURE AT SUBSTANTIALLY 800* C. FOR AT LEAST ABOUT ONE HOUR, WASHING THE SO-HEATED MATERIAL WITH DILUTE ACID AND THEN WATER TO THEREBY REMOVE UNREACTED ZINC OXIDE FROM THE SO HEATED MATERIAL, MIXING A COPPER ACTIVATOR AND A HALIDE WITH THE SO TREATED MATERIAL, AND HEATING THE SO FORMED MIXTURE IN A NON-REDUCING ATMOSPHERE TO A
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗